    GEN 99 Overview

    GEN 99 is used for GMAW and GTAW welding of cast iron. While the wire is primarily used to repair gray iron castings, it is also used for overlay and buildup. A preheat and interpass temperature of 350oF (175oC) minimum is recommended during welding.

    Welding Wire Reels

    Composición química de AWS (típica)

    %C %Mn %Ni %Cu
    1.0 max
    0.004
    2.5 max
    0.01
    90 min
    99.5
    4.0 max
    0.01
    %Si %Fe %S Total
    0.75 max
    0.11
    4.0 max
    0.15
    0.03 max
    0.001
    1.0 max
    <0.20

    Propiedades mecánicas típicas del metal de soldadura

    Fuerza de Tensión 67,500 psi 465 MPa
    Límite elástico 35,000 psi 241 MPa
    Alargamiento 40 %

    Typical Welding Parameters

    Proceso Diameter Voltage Amperage Gas/Flux
    TIG (GTAW) 1/16” (1.6 mm) 14 – 18 90 – 130 100% Ar
    3/32” (2.4 mm) 15 – 20 120 – 175 100% Ar
    1/8” (3.2 mm) 15 – 20 150 – 220 100% Ar
    MIG (GMAW) .035” (0.9 mm) 29 – 33 160 – 180 75% Ar – 25% He
    .045” (1.1 mm) 29 – 33 180 – 220 75% Ar – 25% He
    .062” (1.6 mm) 29 – 33 200 – 250 75% Ar – 25% He