GEN 208 Overview
GEN 208 is used for TIG, MIG, and SAW welding of nickel 200 or 201. This filler metal is also employed for overlaying on steel as well as repairing cast iron castings. It can also be used for dissimilar joints between nickel or nickel alloys to stainless or ferritic steels. Additionally, GEN 208 is used for surfacing of steel.
Composición química de AWS (típica)
| %C | %Mn | %Ni | %Cu | %Fe | %Al |
|---|---|---|---|---|---|
|
0.15 max. 0.04 |
1.0 max. 0.38 |
93.0 min. 95.50 |
0.25 max. 0.015 |
1.0 max. 0.18 |
1.50 max. 0.10 |
| %Si | %P | %S | %Ti | Total Otros |
|---|---|---|---|---|
|
0.75 max. 0.57 |
0.03 max. 0.003 |
0.015 max. 0.003 |
2.0 – 3.5 2.95 |
0.50 max. |
Propiedades mecánicas típicas del metal de soldadura
| Fuerza de Tensión | 65,000 psi | 448 MPa |
| Límite elástico | 36,000 psi | 248 MPa |
| Alargamiento | 28% |
Typical Welding Parameters
| Proceso | Diameter | Voltage | Amperage | Gas/Flux |
|---|---|---|---|---|
| TIG (GTAW) | 1/16” (1.6 mm) | 14 – 18 | 90 – 130 | 100% Ar |
| 3/32” (2.4 mm) | 15 – 20 | 120 – 175 | 100% Ar | |
| 1/8” (3.2 mm) | 15 – 20 | 150 – 220 | 100% Ar | |
| MIG (GMAW) | .035” (0.9 mm) | 26 – 30 | 150 – 200 | 75% Ar – 25% He |
| .045” (1.1 mm) | 28 – 32 | 170 – 220 | 75% Ar – 25% He | |
| Sub Arc (SAW) | .093” (2.4 mm) | 28 – 31 | 275 – 350 | |
| .125” (3.2 mm) | 29 – 32 | 350 – 450 |