    GEN 208 Overview

    GEN 208 is used for TIG, MIG, and SAW welding of nickel 200 or 201. This filler metal is also employed for overlaying on steel as well as repairing cast iron castings. It can also be used for dissimilar joints between nickel or nickel alloys to stainless or ferritic steels. Additionally, GEN 208 is used for surfacing of steel. 

    Welding Wire Reels

    Chemische Zusammensetzung von AWS (typisch)

    %C %Mn %Ni %Cu %Fe %Al
    0.15 max.
    0.04
    1.0 max.
    0.38
    93.0 min.
    95.50
    0.25 max.
    0.015
    1.0 max.
    0.18
    1.50 max.
    0.10
    %Si %P %S %Ti Insgesamt Andere
    0.75 max.
    0.57
    0.03 max.
    0.003
    0.015 max.
    0.003
    2.0 – 3.5
    2.95
    0.50 max.

    Typische mechanische Eigenschaften von Schweißgut

    Zerreißfestigkeit 65,000 psi 448 MPa
    Ertragsstärke 36,000 psi 248 MPa
    Verlängerung 28%

    Typical Welding Parameters

    Verfahren Diameter Voltage Amperage Gas/Flux
    WIG (GTAW) 1/16” (1.6 mm) 14 – 18 90 – 130 100% Ar
    3/32” (2.4 mm) 15 – 20 120 – 175 100% Ar
    1/8” (3.2 mm) 15 – 20 150 – 220 100% Ar
    MIG (GMAW) .035” (0.9 mm) 26 – 30 150 – 200 75% Ar – 25% He
    .045” (1.1 mm) 28 – 32 170 – 220 75% Ar – 25% He
    Sub Arc (SAW) .093” (2.4 mm) 28 – 31 275 – 350
    .125” (3.2 mm) 29 – 32 350 – 450